Prepare edits:Silica can be obtained by the rapid oxidation of silicon dioxide with elemental silica at high temperature: SiO2 + Si → 2SiO Use edits:Solid silicon monoxide can be used as insulating materials. If you have a demand for silicon monoxide powder, please feel free to send me an email for quotation.
Features of SiO Silicon Monoxide Powder :
Silicon monoxide is an inorganic compound. Its chemical formula is SiO. It is a dark brown to loess-colored amorphous powder at room temperature and pressure. Its melting point is 1702°C, boiling point is 1880°C, and its density is 2.13g/㎝³. Stable, it will oxidize to silica in the air.
Application of SiO Silicon Monoxide Powder :
Because silicon monoxide fine powder is very active, it can be used as fine ceramic synthetic raw materials, such as silicon nitride and silicon carbide fine ceramic powder raw materials. Used for the preparation of optical glass and semiconductor materials.
Evaporate it in a vacuum and coat it on the metal mirror surface of the optical instrument as a protective film. Preparation of semiconductor materials.
Storage of natural compound graphite powder
Safety
is usually a little detrimental to the water body. Do not expose
undiluted or large quantities of products to groundwater, waterways or
sewerage systems. Do not allow the material to be discharged into the
surrounding environment without the permission of the government.
At room temperature under normal pressure to avoid light, open flame, high temperature.
Room temperature sealed dark, ventilated and dry place.
Silicon monoxide Health & Safety Information | |
Safety Warning | Danger |
Hazard Statements | H314-H335 |
Hazard Codes | Xi |
Risk Codes | R36/37/38 |
Safety Statements | 26/36 |
RTECS Number | N/A |
Transport Information | N/A |
WGK Germany | N/A |
Silicon Monoxide Properties | |
Other Names | Siliconmonoxidepowder |
CAS No. | 10097-28-6 |
Compound Formula | SiO |
Molecular Weight | 44.08 |
Appearance | black or pale yellow powder |
Melting Point | 1702°C |
Boiling Point | 1880°C |
Density | 2.13g/㎝³ |
Solubility in H2O | N/A |
Electrical Resistivity | N/A |
Refractive index | 1.980 |
Specific Heat | N/A |
Thermal Conductivity | N/A |
Thermal Expansion | N/A |
Young's Modulus | N/A |
Exact Mass | N/A |
Monoisotopic Mass | N/A |
Artificial Graphite YXA-H for Energy Storage Battery materials meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a dem
Artificial Graphite YXA-H2 for Energy Storage Battery materials meet all power specifications including high capacity (about 346.3mAh/g) and high first cycle efficiency (about 95.9%). If you have a de
Artificial Graphite H9 for Power Lithium Battery materials meet all power specifications including high capacity (about 354.9mAh/g) and high first cycle efficiency (about 95.3%). If you have a demand
Artificial Graphite HC15 for Power Lithium Battery materials meet all Power specifications including high capacity (about 354.4mAh/g) and high first cycle efficiency (about 95.4%). If you have a deman
GS-16 Modified artificial graphite meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a demand for GS-16 Modified artif
SYC-1 Silicon-Carbon Anode Materials, Lithium Graphite Battery meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a dem
Anthracite artificial graphite, Graphite Particle Size meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a demand for
Anthracite Artificial Graphite Powder meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a demand for Particle Size 681
Artificial compound graphite meet all power specifications including high capacity (about 346.8mAh/g) and high first cycle efficiency (about 95.9%). If you have a demand for artificial compound graphi
Prepare edits:Silica can be obtained by the rapid oxidation of silicon dioxide with elemental silica at high temperature: SiO2 + Si → 2SiO Use edits:Solid silicon monoxide can be used as insulating ma
In the Si/C composite system, Si particles serve as the active material to provide lithium storage capacity. C can not only buffer the volume change of the silicon anode during the discharge process,
Natural Graphite 216-3 for 18650 Lithium-ion Battery Anode materials meet all required specifications including high capacity (>358 mAh/g) and high first cycle efficiency (95%). If you have a demand f
Artificial Graphite GS16-Q for Digital Products Large Capacity Lithium-ion Battery materials meet all digital products specifications including high capacity (about 359.3 mAh/g) and high first cycle e
Artificial Graphite H5 for Power Tool Lithium Battery materials meet all Power Tool specifications including high capacity (about 354.4 mAh/g) and high first cycle efficiency (about 95.4%). If you hav
Artificial Graphite GS16-S for Digital Products Large Capacity Lithium-ion Battery materials meet all digital products specifications including high capacity (about 357 mAh/g) and high first cycle eff